Frequently asked questions
Answers to the questions we are asked most about XRD and XRF testing: what the techniques measure, how much sample to send, how to send it, and how long results take.
Techniques and materials
What is the difference between XRF and XRD?
XRF identifies and quantifies elements, roughly fluorine to uranium, in percent or parts per million. XRD is the most direct method for identifying crystalline compounds and their percentages. Using both together improves phase identification and quantification.
Are XRD and XRF destructive to my sample?
No. Both generally need a powdered sample, ground to about 50 microns or finer.
What materials can be tested?
Nearly any solid. That includes natural materials such as soil, rock, clay and coal, and industrial materials such as residues, scale, cement and ceramic process materials.
Can XRD always identify what is in the sample?
Usually, but not always. Samples with high amorphous content or overlapping peaks can be hard to identify. In those cases XRF, SEM or FTIR can help.
What method do you use to identify clay minerals?
We follow USGS guidelines, including glycolation and heat treatments at 400°C and 550°C. Kaolinite can be distinguished from chlorite, and from halloysite if needed.
Sample requirements
How much sample is required?
It depends on the test. Routine XRD needs about 1 g.
| Test | Sample size |
|---|---|
| XRD, crystalline minerals | About 1 g. Milligram samples on a low-background holder. |
| XRD, clay analysis | About 20–60 g, depending on clay content |
| XRF, major elements | About 0.4–5 g of powder |
| XRF, trace and semi-quantitative | About 2–5 g |
| Loss on ignition (LOI) | About 5 g |
| Laser particle sizing | About 1–20 g, depending on particle count and size |
| Petrography | A fist-sized sample is ideal. Standard thin sections are 75 × 26 mm. |
| SEM | Chip-sized, 15 mm or less. Must withstand vacuum. Resin mounting is optional. Samples are coated with a conductive material. |
Can you perform XRD analysis with less sample?
Yes. Zero-background holders can accept milligram-sized samples.
Submission and shipping
How do I submit samples?
Notify the lab by email or phone before sending. Include a purchase order or test request form listing sample numbers and test requirements. Label your samples, then seal and package them properly.
Attn: Lab ManagerSietronics Pty Ltd
40 Hoskins Street
Mitchell ACT 2911, Australia
+61 2 6246 9299
Can you accept samples from overseas?
Yes, from almost all countries. Contact the lab before shipping to learn how to pack your samples and what information to include. Some samples may need to be gamma irradiated on entry to Australia.
Turnaround, reports and pricing
How long do results take?
XRD results take 1–2 weeks from receipt. Results in 24–48 hours may be available for an extra charge.
| Test | Turnaround from receipt |
|---|---|
| XRD | 1–2 weeks (24–48 hours expedited, extra charge) |
| XRF | 2–3 weeks |
| Particle sizing | 1–2 weeks |
| Petrology | 4–6 weeks |
| SEM | Depends on the application |
How are results delivered?
As a PDF report. For XRD and chemistry, the data is also supplied in XLSX format.
Are there template reports?
Yes. Example reports are available on the Downloads page.
Do you offer discounts for large batches?
Yes. Discounts are available for bulk sample submissions. Ask when you request a quote.
Do you offer discounts for ongoing work?
Yes. Discounts are available on ongoing jobs. Tell us the expected volume and frequency when you enquire.
Request a quote
Tell us what the samples are and what you need to know. If you are unsure which test fits, describe the problem and we will recommend one.
+61 2 6246 9299 lab@sietronics.com.au 40 Hoskins Street, Mitchell ACT 2911